ФЕРИТНИ EFD ЯДРА

|
МОДЕЛ |
G.W |
РАЗМЕР (mm) |
|||||||
|
A |
B |
C |
D |
C |
F |
G |
H |
||
|
EFD20 |
9 |
20.0±0.6 |
15.4±0.5 |
8.9±0.2 |
6.7±0.2 |
7.7±0.3 |
10.0±0.3 |
0.2±0.1 |
3.6±0.2 |
|
EFD21A |
9 |
20.8±0.6 |
15.4мин |
8.9±0.2 |
6.7±0.2 |
7.7±0.3 |
10.0±0.3 |
0.2±0.1 |
3.6±0.2 |
|
EFD21B |
9.7 |
21.0±0.5 |
15.4мин |
8.9±0.2 |
6.7±0.2 |
8.0±0.3 |
10.3±0.3 |
\ |
3.6±0.2 |
|
EFD25.6 |
19 |
25.6±0.7 |
19.5±0.7 |
11.4±0.3 |
9.1±0.3 |
9.3±0.3 |
12.5±0.3 |
0.6±0.1 |
5.2±0.3 |
|
EFD31 |
25 |
30.8±0.8 |
23.2мин |
14.4±0.3 |
8.8±0.2 |
11.2±0.3 |
15.0±0.3 |
0.3±0.2 |
4.8±0.2 |
|
EFD34 |
29.6 |
34.0±0.6 |
24.0±0.5 |
17.0±0.3 |
5.0±0.2 |
18.0±0.3 |
23.0±0.3 |
\ |
3.0±0.2 |
|
EFD40/45/11 |
60 |
40.5±0.7 |
30.0 мин |
16.6±0.3 |
10.6±0.2 |
16.3±0.3 |
22.5±0.3 |
\ |
6.6±0.2 |
|
EFD40/44/8 |
44 |
40.0±0.7 |
29.5мин |
19.9±0.4 |
8.0±0.2 |
17.1±0.3 |
22.0±0.3 |
\ |
4.0±0.2 |
|
EFD43/53/4.4 |
63.6 |
43.0±0.8 |
28.5мин |
21.6±0.4 |
7.6±0.25 |
19.3±0.3 |
26.5±0.3 |
\ |
4.4±0.25 |
|
EFD43/44/3.2 |
49.2 |
43.4±0.8 |
33.5мин |
22.3±0.4 |
8.0±0.25 |
17.1±0.3 |
22.2±0.3 |
\ |
3.2±0.25 |
|
EFD45/50 |
67 |
45.2±0.8 |
33.3±0.8 |
24.0±0.4 |
7.8±0.2 |
18.0±0.3 |
24.7±0.3 |
\ |
4.0±0.2 |
|
EFD52.5 |
118 |
52.5±1.1 |
39 мин |
22.5±0.4 |
13.0±0.3 |
19.9±0.3 |
27.0±0.3 |
\ |
7.5±0.3 |
|
МОДЕЛ |
ПАРАМЕТЪР |
AL±25%(nH/N^2) |
N.W(g) |
|||
|
C1mm-1 |
Лем |
Аемм2 |
Вемм3 |
ZP40 |
||
|
EFD20 |
1.52 |
47.0 |
31.0 |
1460.0 |
1150 |
7.9 |
|
EFD21A |
1.57 |
49.3 |
31.0 |
1460.0 |
1400 |
7.9 |
|
EFD21B |
1.57 |
49.3 |
31.4 |
1540.0 |
1450 |
8.6 |
|
EFD25.6 |
1.00 |
57.0 |
58.0 |
3300.0 |
2000 |
16.5 |
|
EFD31 |
0.99 |
68.2 |
69.1 |
4712.0 |
2000 |
23.0 |
|
EFD34 |
1.90 |
95.0 |
50.0 |
4750.0 |
1400 |
33.5 |
|
EFD40/45/11 |
1.02 |
108.8 |
106.5 |
10951.0 |
2300 |
55.0 |
|
EFD40/44/8 |
1.35 |
102.8 |
75.5 |
7750.0 |
1700 |
38.0 |
|
EFD43/53/4.4 |
1.14 |
111.3 |
99.8 |
11113.0 |
2000 |
59.0 |
|
EFD43/44/3.2 |
1.41 |
102.0 |
72.1 |
7352.0 |
1500 |
43.0 |
|
EFD45/49 |
1.08 |
108.0 |
97.7 |
10356.2 |
2700 |
60.0 |
|
EFD52.5 |
0.78 |
132.0 |
168.0 |
23250.0 |
2750 |
109.0 |